Nickel Alloy, Corrosion and Heat Resistant, Forgings 57Ni 19.5Cr 13.5Co 4.3Mo 3.0Ti 1.4Al 0.05Zr 0.006B, Consumable Electrode or Vacuum Induction Melted, 1825 to 1900°F (996 to 1038°C) Solution, Stabilization, and Precipitation Heat Treated
Document status: Active
Nickel Alloy, Corrosion and Heat Resistant, Forgings 57Ni - 19.5Cr - 13.5Co - 4.6Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1825 to 1900 °F (996 to 1038 °C) Solution, Stabilization, and Precipitation Heat Treated
Document status: Active
STEEL BARS AND FORGINGS, CORROSION AND HEAT RESISTANT 2.5Si - 12.8Cr - 8.0Ni Annealed
Document status: Active
Steel, Corrosion and Heat Resistant, Bars and Forgings 2.5si 12.5si 8.0ni Annealed
Document status: Active
Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 57Ni 19.5Cr 13.5Co 4.3Mo 3.0Ti 1.4Al 0.006B 0.05Zr Consumable Electrode or Vacuum Induction Melted 1825 to 1900°F Solution Heat Treated
Document status: Active
Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 57Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.006B - 0.05Zr Consumable Electrode or Vacuum Induction Melted 1825 to 1900 °F Solution Heat Treated
Document status: Active
Nickel Alloy, Corrosion and Heat Resistant, Bars, Forgings and Rings 58Ni 19.5Cr 13.5Co 4.3Mo 3.0Ti 1.4Al 0.05Zr 0.006B Consumable Electrode or Vacuum Induction Melted 1825 to 1900°F (996 to 1038°C) Solution, Stabilization, and Precipitation Heat Treated
Document status: Active
Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 57Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode Remelted or Vacuum Induction Melted 1825 to 1900 oF (996 to 1038 oC) Solution, Stabilization, and Precipitation Heat Treated
Document status: Active
Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, Rings, and Forging Stock 57Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode Remelted or Vacuum Induction Melted 1825 to 1900 °F (996 to 1038 °C) Solution, Stabilization, and Precipitation Heat Treated
Document status: Active
Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 58Ni 19.5Cr 13.5Co 4.3Mo 3.0Ti 1.4Al Consumable Electrode or Vacuum Induction Melted 1975°F (1079°C) Solution Heat Treated
Document status: Active