POLYAMIDE (PA6,6) 25% GLASS FIBER / MINERAL REINFORCED HEAT STABILIZED MOLDING COMPOUND, 75% PCR/PIR CONTENT *** TO BE USED WITH FORD WSS-M99P1111-A***
Document status: [ Active ]
ACRYLONITRILE BUTADIENE STYRENE (ABS) MOLDING COMPOUND, 70 % RECYCLED MATERIAL BY WEIGHT ***TO BE USED WITH FORD WSS-M99P1111-A***
Document status: [ Active ]
POYLAMIDE (PA) 6 HEAT STABILIZED, IMPACT MODIFIED 35% GLASS FIBER REINFORCED MOLDING COMPOUND 65% RECYCLED MATERIAL BY WEIGHT ***TO BE USED WITH FORD WSS-M99P1111-A***
Document status: [ Active ]
POLYBUTYLENE TEREPHTHALATE (PBT), POLYETHYLENE TEREPHTHALATE (PET), HEAT STABILIZED, 50% GLASS FIBER REINFORCED MOLDING COMPOUND, 18% PCR CONTENT ***TO BE USED WITH FORD WSS-M99P1111-A***
Document status: [ Active ]
POLYBUTYLENE TEREPHTHALATE (PBT), POLYETHYLENE TEREPHTHALATE (PET), HEAT STABILIZED, 50% GLASS FIBER REINFORCED MOLDING COMPOUND, 18% PCR CONTENT ***TO BE USED WITH FORD WSS-M99P1111-A***
Document status: [ Revised ]
POLYCARBONATE/ ACRYLONITRILE BUTADIENE STYRENE BLEND (PC+ABS) MOLDING COMPOUND, 65% RECYCLED MATERIAL BY WEIGHT ***TO BE USED WITH FORD WSS-M99P1111-A***
Document status: [ Active ]
POLYESTER MOLDING COMPOUND (PBT+PET), 40% GLASS/MINERAL FILLED, MOLDED-IN-COLOR, INTERIOR, 25% PCR RESIN CONTENT, 15% RECYCLED MATERIAL BY WEIGHT ***TO BE USED WITH FORD WSS-M99P1111-A***
Document status: [ Active ]
POLYESTER MOLDING COMPOUND (PBT+PET), 40% GLASS/MINERAL FILLED, MOLDED-IN-COLOR, INTERIOR, 25% PCR RESIN CONTENT, 15% RECYCLED MATERIAL BY WEIGHT ***TO BE USED WITH FORD WSS-M99P1111-A***
Document status: [ Revised ]
POLYPROPYLENE (PP), 40% MINERAL FILLED, INJECTION MOLDING COMPOUND, RECYCLED WITH 25% PCR AND/OR PIR CONTENT ***TO BE USED WITH FORD WSS-M99P1111-A***
Document status: [ Revised ]
POLYPROPYLENE (PP), 40% MINERAL FILLED, INJECTION MOLDING COMPOUND, RECYCLED WITH 25% PCR AND/OR PIR CONTENT ***TO BE USED WITH FORD WSS-M99P1111-A***
Document status: [ Revised ]