Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, and Rings and Stock for Forgings and Rings 74Ni - 15.5Cr - 8.0Fe
Document status: Active
Nickel Alloy, Corrosion and Heat Resistant, Bars, Forgings, Extrusions, and Rings 62Ni 21.5Cr 9.0Mo 3.65(Cb+Ta) Annealed ( Reaffirmed: Jul 2012 )
Document status: Active
Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, Extrusions, and Rings 62Ni - 21.5Cr - 9.0Mo - 3.65 Cb (Nb) Annealed
Document status: Active
Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, Extrusions, Rings, and Stock for Forgings, Extrusions, and Rings 62Ni - 21.5Cr - 9.0Mo - 3.65Cb (Nb) Annealed
Document status: Active
Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 72Ni - 15.5Cr - 0.95Cb - 2.5Ti - 0.70Al - 7.0Fe Equalized, Precipitation Hardenable
Document status: Active
Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 72Ni - 15.5Cr - 0.95Cb - 2.5Ti - 0.70Al - 7.0Fe Equalized, Precipitation Hardenable
Document status: Active
Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 72Ni - 15.5Cr - 7.0Fe - 2.5Ti - 1.0Cb (Nb) - 0.70Al 2100 ¿¿F (1149 ¿¿C) Solution and Precipitation Heat Treated
Document status: Active
Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 72Ni - 15.5Cr - 7.0Fe - 2.5Ti - 1.0Cb (Nb) - 0.70Al 2100 °F (1149 °C) Solution and Precipitation Heat Treated
Document status: Active
Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, Rings, and Forging Stock 72Ni - 15.5Cr - 7.0Fe - 2.5Ti - 1.0Cb (Nb) - 0.70Al (X750) 2100 °F (1149 °C) Solution and Precipitation Heat Treated
Document status: Active
Alloy Bars, Corrosion and Heat Resistant, Nickel Base - 15.5Cr - 0.95 (Cb + Ta) - 2.5Ti - 0.70Al - 7.0Fe, Consumable Electrode or Vacuum Induction Melted
Document status: Active