Steel Bars and Forgings, Corrosion and Heat Resistant 13.5cr 26ni 3mo 1.8ti
Document status: Active
Steel, Corrosion and Heat-Resistant, Bars, Wire, Forgings, and Tubing 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V Consumable Electrode Melted, 1650 °F (899 °C) Solution Heat Treated
Document status: Active
Steel, Corrosion- and Heat-Resistant, Bars, Wire, Forgings, Mechanical Tubing, and Stock for Forging and Heading, 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V (Alloy A286), Consumable Electrode Remelted, 1650 °F (899 °C) Solution Heat Treated
Document status: Active
Steel Bars, Forgings, Tubing, And Rings, Corrosion And Heatresistant 15cr - 26ni - 1.3mo - 2.1ti - 0 (Cancelled: Jun 1952)
Document status: [ Withdrawn ]
STEEL BARS, FORGINGS, TUBING, AND RINGS, CORROSION AND HEAT RESISTANT 15Cr - 26Ni - 1.3Mo - 2.1Ti - 0.30V 1800° F (982.2° C) Solution and Precipitation Heat Treated
Document status: Active
Steel Bars, Forgings, Tubing, and Rings, Corrosion and Heat Resistant 15Cr 26Ni 1.3Mo 2.1Ti 0.30V 1800°F (982°C) Solution Heat Treated
Document status: Active
Steel, Corrosion and Heat-Resistant, Bars, Wire, Forgings, and Tubing 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V Consumable Electrode Melted 1650 °F (899 °C) Solution and Precipitation Heat Treated
Document status: Active
Steel, Corrosion- and Heat-Resistant, Bars, Wire, Forgings, Mechanical Tubing, and Stock for Forging and Heading 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V (A286) Consumable Electrode Remelted 1650 °F (899 °C) Solution and Precipitation Heat Treated
Document status: Active
Steel, Corrosion-Resistant, Bars and Wire 18Cr - 9Ni (SAE 30303F) Free Machining, High Yield Strength Solution Heat Treated and Cold Worked
Document status: Active
Steel, Corrosion Resistant, Bars and Wire 18Cr - 9Ni (303F) Free Machining, High Yield Strength Solution Heat Treated and Cold Worked
Document status: Active