Name:
DNV GL SHIP TECHNOLOGY I-1-5A PDF
Published Date:
01/01/2016
Status:
[ Active ]
Publisher:
DNV
General
The requirements for application of steel with yield strength of 460 N/mm2 as well as the requirements for extremely thick plates of different yield strength are provided in DNV GL Rules SHIP Pt.5 Ch.2 Sec.10.
Deviating from DNV GL Rules Pt.5 Ch.2 Sec.10 the fatigue assessment shall be carried in accordance with GL Structural Rules for Container Ships (I-1-5), Section 20.
| Edition : | 16 |
| File Size : | 1 file , 160 KB |
| Number of Pages : | 4 |
| Published : | 01/01/2016 |