SAE AMS4236B PDF

SAE AMS4236B PDF

Name:
SAE AMS4236B PDF

Published Date:
08/01/2007

Status:
Active

Description:

Aluminum Alloy, Castings 4.6Cu 0.35Mn 0.25Mg 0.22Ti (A206.0-T4) Solution Heat Treated and Naturally Aged

Publisher:
SAE International

Document status:
Active

Format:
Electronic (PDF)

Delivery time:
10 minutes

Delivery time (for Russian version):
200 business days

SKU:

Choose Document Language:
$21
Need Help?
Primarily for components requiring high strength combined with good ductility and impact strength. Certain design and processing procedures may cause these castings to become susceptible to stress-corrosion cracking.
File Size : 1 file , 94 KB
Note : This product is unavailable in Ukraine, Russia, Belarus
Published : 08/01/2007

History

SAE AMS4236C
Published Date: 02/12/2013
Aluminum Alloy Castings, 4.6Cu - 0.35Mn - 0.25Mg - 0.22Ti (A206.0-T4), Solution Heat Treated and Naturally Aged
$21
SAE AMS4236B
Published Date: 08/01/2007
Aluminum Alloy, Castings 4.6Cu 0.35Mn 0.25Mg 0.22Ti (A206.0-T4) Solution Heat Treated and Naturally Aged
$21

Related products

SAE AS1414A
Published Date: 05/24/2018
PROPELLER SHAFT END - FLANGED 5.125(130.175) BOLT CIRCLE (Stabilized: May 2018)
$12.3
SAE AMS3374G
Published Date: 05/22/2023
Sealing Compound Aircraft Firewall, Silicone
$24.9
SAE J1587_201301
Published Date: 01/04/2013
Electronic Data Interchange Between Microcomputer Systems in Heavy-Duty Vehicle Applications (Stabilized: Jan 2013)
$52.8
SAE AS6479
Published Date: 12/18/2020
Splicer, Fusion, Fiber Optic, Aerospace
$45.9

Best-Selling Products

Process Plant Commissioning : A User Guide
Published Date: 01/01/1990
$25.146