Description:

Titanium Alloy Sheet, Strip, and Plate 6Al 6V 2Sn Solution Heat Treated

Publisher:
SAE International

Document status:
Active

Format:
Electronic (PDF)

Delivery time:
10 minutes

Delivery time (for Russian version):
200 business days

SKU:

Choose Document Language:
$19.8
Need Help?
This specification covers a titanium alloy in the form of sheet, strip, and plate.

This material has been used typically for parts to be formed or machined in the solution heat treated condition and subsequently precipitation heat treated requiring high strength-to-weight ratio and stability up to 550 \mDF (288 \mDC) in the precipitation heat treated condition, but usage is not limited to such applications.

Certain processing procedures and service conditions may cause these products to become subject to stress-corrosion cracking; SAE ARP 982 recommends practices to minimize such conditions.
File Size : 1 file , 460 KB
Note : This product is unavailable in Ukraine, Russia, Belarus
Published : 01/01/2008

History

SAE AMS4988E
Published Date: 12/13/2023
Titanium Alloy Sheet, Strip, and Plate 6Al - 6V - 2Sn Solution Heat Treated
$23.7
SAE AMS4988D
Published Date: 08/08/2018
Titanium Alloy Sheet, Strip, and Plate 6Al - 6V - 2Sn Solution Heat Treated
$23.7
SAE AMS4988C
Published Date: 03/07/2014
Titanium Alloy Sheet, Strip, and Plate 6Al - 6V - 2Sn Solution Heat Treated
$21
SAE AMS4988B
Published Date: 02/07/2013
Titanium Alloy Sheet, Strip, and Plate, 6Al - 6V - 2Sn, Solution Heat Treated
$21
SAE AMS4988A
Published Date: 01/01/2008
Titanium Alloy Sheet, Strip, and Plate 6Al 6V 2Sn Solution Heat Treated
$19.8

Related products

SAE AMS4201G
Published Date: 08/20/2020
Aluminum Alloy Plate 6.2Zn - 2.3Cu - 2.2Mg - 0.12Zr (7050-T7651) Solution Heat Treated, Stress Relieved, and Overaged
$20.7
SAE AS24652B
Published Date: 01/17/2023
ELBOW, TUBE - 90°, BULKHEAD, FLARED TUBE UNIVERSAL TO FLARELESS TUBE
$14.7
SAE AMSM6857A
Published Date: 05/15/2006
Magnesium Alloy Castings, Heat Treatment of
$29.4
SAE AS9361B
Published Date: 08/15/2019
NUT, PLAIN, HEXAGON, CHECK, UNS S66286 130 KSI MIN
$12.3

Best-Selling Products

DIN/IEC 212
Published Date: 09/01/1995
Standard Conditions for Use Prior to and During the Testing of Solid Electrical Insulating Materials - GERMAN ONLY
DIN/IEC 60512-2 Amendment 1
Published Date: 08/01/1995
Electromechanical Components for Electronic Equipment - Basic Testing Procedures and Measuring Methods - Part 2: General Examination, Electrical Continuity and Contact Resistance Tests, Insulation Tests and Voltage Stress Tests - GERMAN ONLY
DIN/IEC 60512-2
Published Date: 05/01/1994
Electromechanical Components for Eelectronic Equipment; Basic Testing Procedures and Measuring Methods; Part 2: General Examination, Electrical Continuity and Contact Resistance Tests, Insulation Tests and Voltage Stress Tests - GERMAN ONLY
DIN/IEC 60512-3
Published Date: 05/01/1994
Electromechanical Components for Electronic Equipment; Basic Testing Procedures and Measuring Methods; Part 3: Current-Carrying Capacity Tests - GERMAN ONLY
DIN/IEC 60512-4
Published Date: 05/01/1994
Electromechanical Components for Electronic Equipment; Basic Testing Procedures and Measuring Methods; Part 4: Dynamic Stress Tests - GERMAN ONLY
DIN/IEC 60512-5
Published Date: 05/01/1994
Electromechanical Components for Electronic Equipment; Basic Testing Procedures and Measuring Methods; part 5: Impact Tests (Free Components), Static Load Tests (Fixed Components), Endurance Tests and Overload Tests - GERMAN ONLY