SAE AMS5662B PDF

SAE AMS5662B PDF

Name:
SAE AMS5662B PDF

Published Date:
11/01/1967

Status:
Active

Description:

ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT Nickel Base - 19Cr - 3.1Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al Consumable Electrode or Vacuum Induction Melted 1750 F (954.4 C) Solution Heat Treated

Publisher:
SAE International

Document status:
Active

Format:
Electronic (PDF)

Delivery time:
10 minutes

Delivery time (for Russian version):
200 business days

SKU:

Choose Document Language:
$20.7
Need Help?

FORM: Bars, forgings, flash welded rings, and stock for forgings, flash welded rings, or heading.

APPLICATION: Primarily for parts, such as flanges, cases, and fasteners, requiring high resistance to creep and stress-rupture up to 1300 F (704 C) and oxidation resistance up to 1800 F (982 C), particularly those which are formed or welded and then heat treated to develop required properties.


File Size : 1 file , 93 KB
Note : This product is unavailable in Ukraine, Russia, Belarus
Number of Pages : 6
Published : 11/01/1967

History

SAE AMS5662P
Published Date: 08/17/2022
Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, Rings, and Stock for Forgings and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1775 °F (968 °C) Solution Heat Treated, Precipitation-Hardenable
$27.6
SAE AMS5662M
Published Date: 07/12/2004
Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1775 °F (968 °C) Solution Heat Treated, Precipitation-Hardenable (Reaffirmed 2009)
91.00 81.00 you save 10.00
SAE AMS5662L
Published Date: 07/01/2000
Nickel Alloy, Corrosion and Heat Resistant, Bars, Forgings, and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1775 °F (968 °C) Solution Heat Treated, Precipitation Hardenable
$27.3
SAE AMS5662K
Published Date: 01/01/1998
NICKEL ALLOY, CORROSION AND HEAT RESISTANT, BARS, FORGINGS, AND RINGS 52.5Ni - 19Cr - 3.0Mo - 5.1Cb - 0.90Ti - 0.50AI - 18Fe Consumable Electrode or Vacuum Induction Melted 1775 °F (968°C) Solution Heat Treated, Precipitation Hardenable
$27.3
SAE AMS5662B
Published Date: 11/01/1967
ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT Nickel Base - 19Cr - 3.1Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al Consumable Electrode or Vacuum Induction Melted 1750 F (954.4 C) Solution Heat Treated
$20.7

Related products

SAE AMS3303L
Published Date: 02/27/2019
Elastomer: Silicone, Rubber (MQ/VMQ) General Purpose 55 - 65 Durometer Type "A" Hardness
$22.2
SAE AMS4902M
Published Date: 03/20/2023
Titanium Sheet, Strip, and Plate Commercially Pure Annealed 40.0 ksi (276 MPa) Yield Strength
$22.2

Best-Selling Products